The nanoindentation test is frequently used as an alternate method to obtain the mechanical properties of ductile materials. However. due to the lack of information about the effects of the sample and indenter physical configurations. the accuracy of the extracted material properties in nanoindentation tests requires further evaluation that has been considered in this study. https://www.foldlyers.shop/product-category/toslink/
Effects of Sample and Indenter Configurations of Nanoindentation Experiment on the Mechanical Behavior and Properties of Ductile Materials